Why Palm Oil Mills are Switching from Bronze Bearings to Nylon Plastic?

Analyzing the efficiency of replacing conventional bronze bearings in palm oil mills with Niobush nylon polymer bushings that require no lubrication.

For the past century, Brass and Bronze alloys have been hailed as the gold standard of manufacturing worthiness thanks to their heat conductivity and supporting high shear loads. However, in the palm oil industry (PKS Mills), which is essentially an ocean of hot acid vapor, abrasive mud, and liquid CPO... Bronze often becomes the source of swelling operational costs (OPEX).

3 Reasons PKS Must Discard Bronze

1. Free Fatty Acid (FFA) Corrosion

The biggest challenge for Palm Oil Mills is in the Digester and Screw Press processing environments, which are bathed in high-level organic hot FFA. Bronze is a non-ferrous metal alloy; which means it is very poor when it comes to resisting acid corrosion. Palm acid chemical reactions eat away at the metal shaft structure in a matter of months, peeling micron-after-micron of the copper bushing.

2. Shaft Wear Out Waste

Physics law of friction (galling): if two hard products maneuver together with insufficient lubrication, the hard particles will degrade symmetrically. The use of Solid Bronze will excavate the expensive surface of the steel drive shaft, which in terms of spare part replacement is double the nominal loss.

3. The Grease Pumping Nightmare

Bronze will not maneuver without a thick layer of grease. In conditions of kernel dust, plantation sand, the grease system is very prone to hardening and jamming (seize-up). The routine of workers constantly manual pumping to 50 bronze stations is simply time-inefficient.

Extreme Substitution: Niobush Engineering Plastics

This is where Casting Nylon (PA6G) components come in. This polymer has adaptive true anti-corrosive molecules. Unlike metal, Casting Nylon lasts forever in pools of palm oil acid (FFA).

  • Nylon withstands friction up to a 100 Degree Celsius station terror point without melting into mush.
  • Niobush's slipperiness coefficient is extraordinary. When jamming occurs, this plastic is the one willing to 'Lose' and save the very expensive steel shaft from being ground away.
  • In terms of TCO costs, bulk buying PA6 nylon pipes is proven to be 45% more economical in total funding.

It is highly recommended structurally in PKS, from the Sterilizer station (lorry doors), Kernel elevator support pillars, to digester bottom bearings, to completely switch to NIOBUSH Cast Nylon material specifications.

Have Specific Questions?

Our team of engineers is ready to help provide specific guidance for your agricultural, manufacturing, and palm oil machinery needs.